Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: http://earchive.tpu.ru/handle/11683/139848
Полная запись метаданных
Поле DCЗначениеЯзык
dc.contributor.authorLegostaeva, Elena Viktorovnaen
dc.contributor.authorEroshenko, Anna Yurjevnaen
dc.contributor.authorVavilov, Vladimir Platonovichen
dc.contributor.authorSkripnyak, Vladimir Albertovichen
dc.contributor.authorLuginin, Nikita Andreevichen
dc.contributor.authorChulkov, Arseniy Olegovichen
dc.contributor.authorKozulin, Aleksandr Anatoljevichen
dc.contributor.authorSkripnyak, Vladimir Vladimirovichen
dc.contributor.authorSchmidt, Jurgenen
dc.contributor.authorTolmachev, Aleksey Ivanovichen
dc.contributor.authorUvarkin, Pavel Viktorovichen
dc.contributor.authorSharkeev, Yury Petrovichen
dc.date.accessioned2026-11-27T09:45:33Z-
dc.date.available2026-11-27T09:45:33Z-
dc.date.issued2023-
dc.identifier.citationInfluence of Severe Plastic Deformation by Extrusion on Microstructure, Deformation and Thermal Behavior under Tension of Magnesium Alloy Mg-2.9Y-1.3Nd / Elena Legostaeva, Anna Eroshenko, Vladimir Vavilov [et al.] // Metals. — 2023. — Vol. 13, iss. 5. — Article number 988, 17 p..en
dc.identifier.urihttp://earchive.tpu.ru/handle/11683/139848-
dc.description.abstractThe microstructural investigation, mechanical properties, and accumulation and dissipation of energies of the magnesium alloy Mg-2.9Y-1.3Nd in the recrystallized state and after severe plastic deformation (SPD) by extrusion are presented. The use of SPD provides the formation of a bimodal structure consisting of grains with an average size 15 µm and of ultrafine-grained grains with sizes less than 1 µm and volume fractions up to 50%, as well as of the fine particles of the second Mg24Y5 phases. It is established that grain refinement during extrusion is accompanied by an increase of the yield strength, increase of the tensile strength by 1.5 times, and increase of the plasticity by 1.8 times, all of which are due to substructural hardening, redistribution of the phase composition, and texture formation. Using infrared thermography, it was revealed that before the destruction of Mg-2.9Y-1.3Nd in the recrystallized state, there is a sharp jump of temperature by 10 °C, and the strain hardening coefficient becomes negative and amounts to (−6) GPa. SPD leads to a redistribution of thermal energy over the sample during deformation, does not cause a sharp increase in temperature, and reduces the strain hardening coefficient by 2.5 timesen
dc.format.mimetypeapplication/pdf-
dc.language.isoenen
dc.publisherMDPI AGen
dc.relation.ispartofMetals. 2023. Vol. 13, iss. 5en
dc.rightsinfo:eu-repo/semantics/openAccess-
dc.rightsAttribution-NonCommercial 4.0 Internationalen
dc.rights.urihttps://creativecommons.org/licenses/by-nc/4.0/-
dc.sourceMetalsen
dc.subjectэлектронный ресурсru
dc.subjectтруды учёных ТПУru
dc.subjectMg-based bioinert alloysen
dc.subjectultrafine-grained stateen
dc.subjectsevere plastic deformationen
dc.subjectmicrostructureen
dc.subjectmechanical propertiesen
dc.titleInfluence of Severe Plastic Deformation by Extrusion on Microstructure, Deformation and Thermal Behavior under Tension of Magnesium Alloy Mg-2.9Y-1.3Nden
dc.typeArticleen
dc.typeinfo:eu-repo/semantics/article-
dc.typeinfo:eu-repo/semantics/publishedVersion-
dcterms.audienceResearchesen
local.filepathreprint-685115.pdf-
local.filepathhttps://doi.org/10.3390/met13050988-
local.identifier.bibrec(RuTPU)685115-
local.issue5-
local.localtypeСтатьяru
local.volume13-
dc.identifier.doi10.3390/met13050988-
Располагается в коллекциях:Репринты научных публикаций

Файлы этого ресурса:
Файл РазмерФормат 
reprint-685115.pdf4,33 MBAdobe PDFПросмотреть/Открыть


Лицензия на ресурс: Лицензия Creative Commons Creative Commons