Название: | Preceramic Paper-Derived SiCf/SiCp Composites Obtained by Spark Plasma Sintering: Processing, Microstructure and Mechanical Properties |
Авторы: | Li Ke Kashkarov, Egor Borisovich Syrtanov, Maksim Sergeevich Sedanova, Elizaveta Pavlovna Ivashutenko, Alexander Sergeevich Lider, Andrey Markovich Fan Ping Yuan Daqing Travitsky, Nakhum |
Ключевые слова: | керамические композиты; карбид кремния; спекание; компьютерная томография; микроструктура; ceramic matrix composites; preceramic paper; silicon carbide; fibers; spark plasma sintering; small punch test; X-ray computed tomography; microstructure; mechanical properties |
Дата публикации: | 2020 |
Издатель: | MDPI AG |
Библиографическое описание: | Preceramic Paper-Derived SiCf/SiCp Composites Obtained by Spark Plasma Sintering: Processing, Microstructure and Mechanical Properties / Li Ke, E. B. Kashkarov, M. S. Syrtanov [et al.] // Materials. — 2020. — Vol. 13 iss. 3. — [607, 14 p.]. |
Аннотация: | Ceramic matrix composites (CMCs) based on silicon carbide (SiC) are promising materials for applications as structural components used under high irradiation flux and high temperature conditions. The addition of SiC fibers (SiCf) may improve both the physical and mechanical properties of CMCs and lead to an increase in their tolerance to failure. This work describes the fabrication and characterization of novel preceramic paper-derived SiCf/SiCp composites fabricated by spark plasma sintering (SPS). The sintering temperature and pressure were 2100 °C and 20–60 MPa, respectively. The content of fibers in the composites was approx. 10 wt.%. The matrix densification and fiber distribution were examined by X-ray computed tomography and scanning electron microscopy. Short processing time avoided the destruction of SiC fibers during SPS. The flexural strength of the fabricated SiCf/SiCp composites at room temperature varies between 300 and 430 MPa depending on the processing parameters and microstructure of the fabricated composites. A quasi-ductile fracture behavior of the fabricated composites was observed. |
URI: | http://earchive.tpu.ru/handle/11683/64957 |
Располагается в коллекциях: | Репринты научных публикаций |
Файлы этого ресурса:
Файл | Описание | Размер | Формат | |
---|---|---|---|---|
reprint-nw-33265.pdf | 3,08 MB | Adobe PDF | Просмотреть/Открыть |
Лицензия на ресурс: Лицензия Creative Commons