Please use this identifier to cite or link to this item: http://earchive.tpu.ru/handle/11683/33917
Title: On Quality of a Weld Bead Using Power Wire 35v9h3sf
Authors: Kozyrev, N. A.
Galevskiy, G. V.
Titov, D. A.
Kolmogorov, Dmitry Evgenievich
Gusarov, D. E.
Keywords: сварные швы; силовые провода; порошковые проволоки; твердость; микротвердость; порошковые смеси; никель; неметаллические включения; слои
Issue Date: 2016
Publisher: IOP Publishing
Citation: On Quality of a Weld Bead Using Power Wire 35v9h3sf / N. A. Kozyrev [et al.] // IOP Conference Series: Materials Science and Engineering. — 2016. — Vol. 125 : Materials Treatment: Current Problems and Solutions : All-Russia Scientific and Practical Conference, 26–28 November 2015, Yurga, Russia : [proceedings]. — [012028, 7 p.].
Abstract: The effect of introducing carbon-fluorine containing additives and nickel to flux-cored wire 35V9H3SF on its structure, micro hardness of martensite, hardness and wear rate of a welded layer has been investigated. It has been proven that carbon-fluorine additions to a powder mixture increase the hardness of the deposited layer and its wearing strength. Nickel adding increases the hardness of both martensite and the deposited layer, and reduces abrasion wear. Introducing carbon-fluorine containing additives to the powder mixture can reduce the pore formation and lower the level of impurity with nonmetallic inclusions; and nickel adding can lead to austenite having a finer grain size.
URI: http://earchive.tpu.ru/handle/11683/33917
Appears in Collections:Материалы конференций

Files in This Item:
File Description SizeFormat 
dx.doi.org-10.1088-1757-899X-125-1-012028.pdf7,37 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.