Название: Investigative study of the radiation damage on fuel clad of miniature neutron source reactor using computational tools
Авторы: Alkhassan, Samiru
Belyavsky, Sergey Vladimirovich
Nesterov, Vladimir Nikolaevich
Дата публикации: 2021
Издатель: IOP Publishing Ltd.
Библиографическое описание: Alkhassan, S. Investigative study of the radiation damage on fuel clad of miniature neutron source reactor using computational tools / S. Alkhassan, S. V. Belyavsky, V. N. Nesterov // Journal of Physics: Conference Series. — Bristol : IOP Publishing Ltd., 2021. — Vol. 2064 : Gas Discharge Plasmas and Their Applications (GDP 2021) : 15th International Conference, 5-10 September 2021, Ekaterinburg, Russia. — [ 012103, 6 p.].
Аннотация: Core conversion requires some evaluation of the reactor safety. Changes to the reactivity worth, shutdown margin, power density and material properties are crucial to the proper functioning of the reactor. The focus of this article is to study the neutron flux distribution in the reactor core and radiation damage on candidate clads. The Ghana Research Reactor-1 (GHARR-1) operates at maximum power of 30 kW in order to attain a flux of 1.0? 1012 n·cm–2·s for the high enriched uranium core. Using the GHARR-1 core geometry, considering 348 fuel pins, the multiplication factor (Keff) is calculated at enrichments of 10%, 12.5%, 16%, 20%, 30% and 90.2%. The spectrum of neutron flux generated in the 26 group is also calculated at the specified enrichments. The ion/particle interactions with the targets (clad) were studied in the Stopping and Range of Ion in Matter code to establish the best clad material based on recorded defects and vacancies generated. From the calculations and simulations, the best choice from the candidate clads based on the assessment is SiC. The calculation of the fuel campaign length gives 7.5 years. The defects sustained by the prospective clad showed low susceptibility to swelling and other forms of deformation.
URI: http://earchive.tpu.ru/handle/11683/72799
Располагается в коллекциях:Репринты научных публикаций

Файлы этого ресурса:
Файл Описание РазмерФормат 
conf-nw-39154.pdf1,12 MBAdobe PDFПросмотреть/Открыть


Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.