Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс:
http://earchive.tpu.ru/handle/11683/139823Полная запись метаданных
| Поле DC | Значение | Язык |
|---|---|---|
| dc.contributor.author | Rusin, Nikolay Martemjyanovich | en |
| dc.contributor.author | Skorentsev, Aleksandr Leonidovich | en |
| dc.contributor.author | Akimo, Kirill Olegovich | en |
| dc.contributor.author | Likharev, Vadim Evgenjevich | en |
| dc.contributor.author | Ilyashchenko, Dmitry Pavlovich | en |
| dc.contributor.author | Dmitriev, Vladimir Ivanovich | en |
| dc.date.accessioned | 2026-11-20T14:02:49Z | - |
| dc.date.available | 2026-11-20T14:02:49Z | - |
| dc.date.issued | 2025 | - |
| dc.identifier.citation | Effect of Laser Energy Density During LPBF on the Structure and Mechanical Properties of Al-15Sn-5Pb Alloy / Nikolay M. Rusin, Alexander L. Skorentsev, Kirill O. Akimov [et al.] // Materials. — 2025. — Vol. 18, iss. 23. — Article number 5268, 11 p.. | en |
| dc.identifier.uri | http://earchive.tpu.ru/handle/11683/139823 | - |
| dc.description.abstract | Al-15Sn-5Pb (vol.%) alloy was fabricated by the Laser Powder Bed Fusion (LPBF) method at laser scanning speeds of 0.8, 1.0, and 1.2 m/s and laser powers ranging from 70 to 130 W. The samples were synthesized from a mixture of elemental powders using an ONSINT AM150 3D printer under a flowing argon atmosphere. The structure and mechanical properties under compression tests of the produced material were investigated as a function of the volumetric laser energy density (E) during LPBF. It has been established that low laser energy density during LPBF results in incomplete melting of aluminum particles and a non-uniform distribution of soft inclusions within the material. Increasing the energy density ensures a significantly more uniform distribution of the phases, resulting in the formation of a fine-grained three-phase alloy. It was established that both the ductility and strength of the alloy improve with the increase in E until a critical value is reached. As a result, at E ≥ 48 J·mm−3, the ultimate strength of the alloy reaches 100 ± 5 MPa, and its deformation before fracture is 15 ± 1%. Substituting one quarter of the tin volume with lead results in a significant increase in the ductility of the LPBF-fabricated aluminum alloy | en |
| dc.format.mimetype | application/pdf | - |
| dc.language.iso | en | en |
| dc.publisher | MDPI AG | en |
| dc.relation.ispartof | Materials. 2025. Vol. 18, iss. 23 | en |
| dc.rights | info:eu-repo/semantics/openAccess | - |
| dc.rights | Attribution-NonCommercial 4.0 International | en |
| dc.rights.uri | https://creativecommons.org/licenses/by-nc/4.0/ | - |
| dc.source | Materials | en |
| dc.subject | laser powder bed fusion (LPBF) | en |
| dc.subject | volumetric laser energy density | en |
| dc.subject | critical energy density | en |
| dc.subject | aluminum matrix alloy | en |
| dc.subject | microstructure; ductility | en |
| dc.subject | compressive strength | en |
| dc.title | Effect of Laser Energy Density During LPBF on the Structure and Mechanical Properties of Al-15Sn-5Pb Alloy | en |
| dc.type | Article | en |
| dc.type | info:eu-repo/semantics/article | - |
| dc.type | info:eu-repo/semantics/publishedVersion | - |
| dcterms.audience | Researches | en |
| local.filepath | reprint-683619.pdf | - |
| local.filepath | https://doi.org/10.3390/ma18235268 | - |
| local.identifier.bibrec | (RuTPU)683619 | - |
| local.issue | 23 | - |
| local.localtype | Статья | ru |
| local.volume | 18 | - |
| dc.identifier.doi | 10.3390/ma18235268 | - |
| Располагается в коллекциях: | Репринты научных публикаций | |
Файлы этого ресурса:
| Файл | Размер | Формат | |
|---|---|---|---|
| reprint-683619.pdf | 4,02 MB | Adobe PDF | Просмотреть/Открыть |
Лицензия на ресурс: Лицензия Creative Commons