Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс:
http://earchive.tpu.ru/handle/11683/139823| Название: | Effect of Laser Energy Density During LPBF on the Structure and Mechanical Properties of Al-15Sn-5Pb Alloy |
| Авторы: | Rusin, Nikolay Martemjyanovich Skorentsev, Aleksandr Leonidovich Akimo, Kirill Olegovich Likharev, Vadim Evgenjevich Ilyashchenko, Dmitry Pavlovich Dmitriev, Vladimir Ivanovich |
| Ключевые слова: | laser powder bed fusion (LPBF); volumetric laser energy density; critical energy density; aluminum matrix alloy; microstructure; ductility; compressive strength |
| Дата публикации: | 2025 |
| Издатель: | MDPI AG |
| Библиографическое описание: | Effect of Laser Energy Density During LPBF on the Structure and Mechanical Properties of Al-15Sn-5Pb Alloy / Nikolay M. Rusin, Alexander L. Skorentsev, Kirill O. Akimov [et al.] // Materials. — 2025. — Vol. 18, iss. 23. — Article number 5268, 11 p.. |
| Аннотация: | Al-15Sn-5Pb (vol.%) alloy was fabricated by the Laser Powder Bed Fusion (LPBF) method at laser scanning speeds of 0.8, 1.0, and 1.2 m/s and laser powers ranging from 70 to 130 W. The samples were synthesized from a mixture of elemental powders using an ONSINT AM150 3D printer under a flowing argon atmosphere. The structure and mechanical properties under compression tests of the produced material were investigated as a function of the volumetric laser energy density (E) during LPBF. It has been established that low laser energy density during LPBF results in incomplete melting of aluminum particles and a non-uniform distribution of soft inclusions within the material. Increasing the energy density ensures a significantly more uniform distribution of the phases, resulting in the formation of a fine-grained three-phase alloy. It was established that both the ductility and strength of the alloy improve with the increase in E until a critical value is reached. As a result, at E ≥ 48 J·mm−3, the ultimate strength of the alloy reaches 100 ± 5 MPa, and its deformation before fracture is 15 ± 1%. Substituting one quarter of the tin volume with lead results in a significant increase in the ductility of the LPBF-fabricated aluminum alloy |
| URI: | http://earchive.tpu.ru/handle/11683/139823 |
| Располагается в коллекциях: | Репринты научных публикаций |
Файлы этого ресурса:
| Файл | Размер | Формат | |
|---|---|---|---|
| reprint-683619.pdf | 4,02 MB | Adobe PDF | Просмотреть/Открыть |
Лицензия на ресурс: Лицензия Creative Commons